* Added K1C and fixed some settings (took from config files instead of Creality Print) * Files renaming * New PLA-CF, prettify json for K1C, naming uniformisation, ... * Port Special PLA profiles to K1/K1 Max * Changed slow down layer time and slow down min speed in order to improve overall speed on details. * Raised PLA bed temp to 55°C * Optimisations for ABS, ASA and added Generic PC profile. * Added PA-CF and fixed PC profiles. * Added new filaments to default materials
52 lines
No EOL
1,023 B
JSON
52 lines
No EOL
1,023 B
JSON
{
|
|
"type": "filament",
|
|
"setting_id": "GFSG99_00",
|
|
"name": "Creality Generic PETG @K1-all",
|
|
"from": "system",
|
|
"instantiation": "true",
|
|
"inherits": "Creality Generic PETG",
|
|
"filament_max_volumetric_speed": [
|
|
"9"
|
|
],
|
|
"slow_down_layer_time": [
|
|
"12"
|
|
],
|
|
"slow_down_min_speed": [
|
|
"20"
|
|
],
|
|
"cool_plate_temp": [
|
|
"70"
|
|
],
|
|
"eng_plate_temp": [
|
|
"70"
|
|
],
|
|
"hot_plate_temp": [
|
|
"70"
|
|
],
|
|
"textured_plate_temp": [
|
|
"70"
|
|
],
|
|
"cool_plate_temp_initial_layer": [
|
|
"70"
|
|
],
|
|
"eng_plate_temp_initial_layer": [
|
|
"70"
|
|
],
|
|
"hot_plate_temp_initial_layer": [
|
|
"70"
|
|
],
|
|
"textured_plate_temp_initial_layer": [
|
|
"70"
|
|
],
|
|
"nozzle_temperature_initial_layer": [
|
|
"250"
|
|
],
|
|
"nozzle_temperature": [
|
|
"250"
|
|
],
|
|
"compatible_printers": [
|
|
"Creality K1C 0.4 nozzle",
|
|
"Creality K1C 0.6 nozzle",
|
|
"Creality K1C 0.8 nozzle"
|
|
]
|
|
} |